Issues with implementation of strain gradient plasticity framework of Niordson and Hutchinson (2003) in Abaqus UEL subroutine
I have implemented the rate-independent strain gradient plasticity framework of Niordson and Hutchinson (2003) in UEL. I was able to validate the results of the shear of infinitely wide thin layer between two rigid surfaces (Niordson and Hutchinson, 2003). However, the UEL subroutine fails to converge for the more complex problem of the shear of finite width slab. I suspect the convergence issues are arising out of internal elastic-plastic boundary conditions and the yield criteria. I have few doubts in this regard.