Studying the Tensile Behaviour of GLARE Laminates: A Finite Element Modelling Approach

Submitted by Payam Soltani on

By: Payam Soltani, M. Keikhosravy & R. H. Oskouei & C. Soutis 

 http://www.springerlink.com/content/h831735260162p66/

Abstract:

Numerical simulations based on finite element modelling are increasingly being

developed to accurately evaluate the tensile properties of GLARE (GLAss fibre REinforced

aluminium laminates). In this study, nonlinear tensile behaviour of GLARE Fibre Metal

Four-year PhD position on modeling of irradiation-induced embrittlement

Submitted by Erik Van der Giessen on

The Micromechanics of Materials group at the Zernike Institute for Advanced Materials in the Netherlands is looking for a qualified PhD student to unravel irradiation-induced embrittlement in nuclear materials. A detailed description can be found in the attachment. Ideally, candidates have an MSc degree in mechanical or nuclear engineering, (applied) physics, material science or a related field, but holders of a BSc with the highest ranks may also be considered.

Apply before it's too late: June 1. 

P as the Optimal Inhibitor for Suppressing Surface Electromigration and Electrical Breakdown at the Source

Submitted by Zhenyu Zhang on

Based on an extensive search across the periodic table utilizing first-principles density functional theory, we discover phosphorus to be an optimal surface electromigration inhibitor on the technologically important Cu(111) surface-the dominant diffusion pathway in modern nanoelectronics interconnects. Unrecognized thus far, such an inhibitor is characterized by energetically favoring (and binding strongly at) the kink sites of step edges. These properties are determined to generally reside in elements that form strong covalent bonds with substrate metal atoms.

Instrumented Indentation, It's More Than Hardness

Submitted by NANOVEA on

As the validity of Instrumented Indentation continues to expand throughout all materials research, many throughout the community are still unclear as to what exactly can be achieved. Although advances in technology will continue to grow the list of capabilities of Instrumented Indentation, we will review a list of what can be expected as of now. But first lets quickly review how Instrumented Indentation works.



The Rodney Hill Prize In Solid Mechanics: call for nominations

Submitted by Dan Lovegrove on

Elsevier Limited has established a prize named The Rodney Hill Prize in Solid Mechanics. This prize, which consists of a plaque and a check for $25,000, is to be awarded in recognition of outstanding research in the field of solid mechanics. The prize is to be awarded every 4 years, to coincide with the quadrennial International Congress of Theoretical and Applied Mechanics (ICTAM). The first prize was awarded at ICTAM 2008 in Adelaide and the second will be awarded at the ICTAM 2012 in Beijing.