Ultrafast Electrochemical Lithiation of Individual Si Nanowire Anodes Submitted by Jianyu Huang on Thu, 05/12/2011 - 18:53 research doping lithium ion battery silicon nanowire fast lithiation carbon coating Nano Letters, DOI: 10.1021/nl200412p Read more about Ultrafast Electrochemical Lithiation of Individual Si Nanowire AnodesLog in to post comments5082 views