Skip to main content

Ruobing Bai's blog

Hydrogel Interferometry for Ultrasensitive and Highly Selective Chemical Detection

Submitted by Ruobing Bai on

Dear Colleagues,

Here you can find our recent paper about hydrogel sensor for chemical detection.

Hydrogel Interferometry for Ultrasensitive and Highly Selective Chemical Detection

Authors: Mo Sun, Ruobing Bai, Xingyun Yang, Jiaqi Song, Meng Qin, Zhigang Suo, Ximin He

Abstract

Fatigue Fracture of Self-Recovery Hydrogels

Submitted by Ruobing Bai on

Dear Colleagues,

Here is our recent paper “Fatigue Fracture of Self-Recovery Hydrogels”. To the hydrogel community, this paper distinguishes the fatigue fracture and the self-recovery of a hydrogel. To the mechanics community, we show that, for the first time in hydrogels, the fatigue threshold depends only on the covalent network, but not on the noncovalent interactions that provide dissipation.

https://pubs.acs.org/doi/abs/10.1021/acsmacrolett.8b00045?journalCode=a…