The effect of film thickness on the failure strain of polymersupported metal films

Submitted by Nanshu Lu on

We perform uniaxial tensile tests on polyimide-supported copper films with a strong (111) fiber texture and with thicknesses varying from 50 nm to 1 μm. Films with thicknesses below 200 nm fail by intergranular fracture at elongations of only a few percent. Thicker films rupture by ductile transgranular fracture and local debonding from the substrate. The failure strain for transgranular fracture exhibits a maximum for film thicknesses around 500 nm.

Disk vs blade natural frequencies

Submitted by cryogene on

I'm trying to determine the coorelation of a blade natural frequency and disk (nodal diameter) natural frequency on a Turbine wheel in ANSYS Modal analysis.  Is it possible for a blade natual frequency to be excited even though a disk natural frequency is not being excited??  I'm having trouble determining if a blade frequency is related to any disk nodal diameter.  Thanks for any incite on this subject.

Two positions for guest researchers(post-doc) at NIST on biomechanics

Submitted by Zhijun Zheng on

 Closed!!!

Two positions for guest researchers(post-doc) at NIST on biomechanics

Email: martin.chiang [at] nist.gov (martin[dot]chiang[at]nist[dot]gov)

Homepage: http://www.nist.gov/msel/polymers/biomaterials/martin_chiang.cfm

Research area: Biomechanics

Practical and graphical remarks about Moving Least Squares

Submitted by Alv on

I have had some time to write down an informal introduction to Moving Least Squares, from my coding perspective. It is supposed to be a condensation of experiences after some years of using it, although it does not contain any new theoretical aspect.

http://www.scribd.com/doc/19409754/yanrMLS

a fracture problem

Submitted by Jin MZ on

  Dear everyone

  If we considerer a 3D fracture stress and strain field as a combination of numerous 2D fields in thickness direction, the J integral at each 2D plane can be obtained according to Rice’s definition (Abaqus and Ansys also include this function). What I concerned is the ratio of J integral at the surface of SEB or CT specimen to that at the mid-plane of the specimen. What factors have influence on the ratio? How to find the quantitive relationship between the factors and the ratio in linear elastic model?

PhD STUDENTSHIPS:FLUID STRUCTURE INTERACTIONS IN MARINE ENGINEERING AND IN BIOINSPIRED DESIGN

Submitted by fhuera on

The Department of Mechanical Engineering at the Universitat Rovira i Virgili (URV) (www.urv.cat) in Tarragona (Spain), is looking for several enthusiastic research students with a strong interest in fluid dynamics. Successful candidates will join a small but very active multidisciplinary team, working in fluid-structure interaction problems. The research will be mainly experimental and focused in the area of fluid structure interaction with application to several engineering problems.

Input Steel Properties in Abaqus

Submitted by looyong on

Hi,

 

I am trying to model a reinforced concrete element in Abaqus. I have been running a couple of models for a few weeks. Recently, I tried to validate an new experiment but ran into this error, "The Plastic Strain At First Yield Should Be Set To Zero". For my steel material model, i used elastic = 29520ksi and for the plastic, i keyed in the yield stress followed by the plastic strain. At the first input, plastic strain is zero for the initial yield stress.