Self-healing materials with microvascular networks
Kathleen S. Toohey, Nancy R. Sottos, Jennifer A. Lewis, Jeffrey S. Moore, and Scott R. White
Self-healing polymers composed of microencapsulated healing agents exhibit remarkable mechanical performance and regenerative ability, but are limited to autonomic repair of a single damage event in a given location. Self-healing is triggered by crack-induced rupture of the embedded capsules; thus, once a localized region is depleted of healing agent, further repair is precluded. Re-mendable polymers can achieve multiple healing cycles, but require external intervention in the form of heat treatment and applied pressure. Here, we report a self-healing system capable of autonomously repairing repeated damage events. Our bio-inspired coating/substrate design delivers healing agent to cracks in a polymer coating via a three-dimensional microvascular network embedded in the substrate. Crack damage in the epoxy coating is healed repeatedly. This approach opens new avenues for continuous delivery of healing agents for self-repair as well as other active species for additional functionality.
For more information see: http://www.mvac.uiuc.edu/network.html
- Nancy Sottos's blog
- Log in or register to post comments
- 6336 reads
Comments
Mechanochemically Active Polymers
Nancy Sottos