Many granular materials encountered in engineering practice are of irregular shapes that are not essentially smooth or rounded. However, in DEM, grains are idealized as spheres and ellipsoids and their surface are assumed to be sufficiently smooth. As a result, I wonder why there is no model of irregular shapes and what is the difficulty on implementing such a model? Is there any recent work aimed to simulate grains of irregular shape? Thanks a lot.
»
- WaiChing Sun's blog
- Log in or register to post comments
- 8047 reads
Comments
The choice of sphere or
The choice of sphere or circle is due to its convenience for contact tracking, which is one of the most time consuming steps in DEM computation. You may cluster spheres or circles to form irregular shapes.
Particle shape in DEM
WaiChing
This recent paper may be of interest
doi:10.1016/j.compgeo.2009.03.001
Potential particles: a method for modelling non-circular particles in DEM
G.T. Houlsby, Comp. geotech.
Regards
Charles
Thanks for the information.
Thanks for the information. It's an interesting paper.