Failure criteria for fabric composite or woven composite
Mon, 2010-04-12 13:16 - Azadeh Sheidaei
Hi All,
Most exisiting failure critera delevolped for fiber composite laminates and they are rough estimations for fabric composite. I want to know if there is a suitable failure criterion for fabric composites.
Thanks
Azadeh
»
- Azadeh Sheidaei's blog
- Log in or register to post comments
- 7117 reads
Comments
Hello Azadeh, As far as I
Hello Azadeh,
As far as I know, some people use multiscale modeling to study the failure behavior of fabric/woven composites.
Failure breaks down into two levels i) microscopic level and ii) macroscopic level. At i) failure criterion for constituents
are considered and the outcome of i) will be transfered into ii) using micro-mechanics.
You may take a look at this reference:
1) R. Rolfes, G. Ernst, M. Vogler and C. Huhne, Material and Failure models for textile composites, in Mechanical Response of Composites., R.R. Camanho, C.G. Davila, S.T. Pinho
J.J.C. Remmers, eds. 2008, Springer, Netherlands
2) and others
Thank you very much.
Thank you very much. specially the first one is very useful.
Azadeh