i am using Deform 3D for my analysis but wats the problem in this software i cant input the material properties,flow stress of the material so the validation with theoritical becomes difficult so if anybody doe know about this how to input the matl pproperties and force of the press please help me

i am designing a die considering it as thick walled cylinder so in order to do this i need to consider the failure criteria so inside is Carbide with 3100 n/mm2 copressive strength and outside is steel casing with 1990mpa yeild strength i know the inside radius of carbide is 10m and pressure is 2973mpa please help