Force is droped during indentation simulation at the step of indenter withdrawal

Submitted by ABAqirl on

Dear All,

I have the following problem. I simulate an indentation in two steps. At first step the indenter penetrate to the material. At the second step it withdraws from it. The problem, at the second step force simply drops, although the behaviour of material is elasto-plastic.. What could be the reason? Incorrect boundary conditions, very soft behaviour of material??? Specialists, please help.

 

Best regards

ABAgirl


it is not very obvious what do you mean by saying  it simply drops?

 

Depending on the ratio sY/E (yield strength over Young's modulus) it may actually simply drop as you say.

 

I think that you are getting the corresct result

 

Mon, 09/05/2011 - 08:29 Permalink

hello Thanasis Zisis,

When i said that the force droped, i means that when the indenter is removing from the body, the force simply decreasing without removing elastic deformation, the relation of SY/E in my case is 0.0074,

What do you think about it?

Best regards

ABAgirl 

Tue, 09/06/2011 - 18:46 Permalink