Submitted by Soumya Laha on Thu, 05/30/2013 - 07:22 Upto what limit is hooke's law really obeyed ? some books say that hooke's law is obeyed up to the proportional limit, while some other books say that hooke's law is upto the elastic limit ? what is the correct answer? Forums Ask iMechanica opinion surajitdas Limit: Hooke,s Law Up to the proportional Limit Hooke,s law is valid. Log in or register to post comments Thu, 05/30/2013 - 09:13 Permalink Log in or register to post comments3408 views
surajitdas Limit: Hooke,s Law Up to the proportional Limit Hooke,s law is valid. Log in or register to post comments Thu, 05/30/2013 - 09:13 Permalink
Limit: Hooke,s Law
Up to the proportional Limit Hooke,s law is valid.