Submitted by juan gomez on Tue, 02/02/2010 - 13:35 Dear Imechanica Members, I am looking for a reference where the concept and definition of Representative Volume Element as the fundamental consitutent of Continuum Mechanics was originally introduced. Thanks in advanced for yoyr help. Juan juan gomez Representative Volume Element (RVE) JUAN GOMEZ PhD Computational Mechanics Professor Applied Mechanics Group EAFIT University Medellin,Colombia Log in or register to post comments Tue, 02/02/2010 - 13:35 Permalink srangan3 In reply to Representative Volume Element (RVE) by juan gomez Hill (JMPS, 1963) Please check the following reference: Hill, R., 1963. Elastic properties of reinforced solids: some theoretical principles. J. Mech. Phys. Solids 11 (5), 357–372. http://www.sciencedirect.com/science?_ob=ArticleURL&_udi=B6TXB-46G500N-… Log in or register to post comments Wed, 02/03/2010 - 03:25 Permalink Ashwani Verma Representative Volume Element constitution dear Imechanica members i am looking for a help how can i constitute representative volume element to study fracture in hetrogeneous alloys. Ashwani Verma Ph D scholar Sant longowal Institute of Engineering & Technology, Longowal (INDIA) Log in or register to post comments Sun, 09/01/2013 - 04:40 Permalink Hua Wang In reply to Representative Volume Element constitution by Ashwani Verma related book there are many works is related to your question. I think you should read the book about micro-mechanics Log in or register to post comments Wed, 09/25/2013 - 13:33 Permalink Log in or register to post comments14521 views
juan gomez Representative Volume Element (RVE) JUAN GOMEZ PhD Computational Mechanics Professor Applied Mechanics Group EAFIT University Medellin,Colombia Log in or register to post comments Tue, 02/02/2010 - 13:35 Permalink
srangan3 In reply to Representative Volume Element (RVE) by juan gomez Hill (JMPS, 1963) Please check the following reference: Hill, R., 1963. Elastic properties of reinforced solids: some theoretical principles. J. Mech. Phys. Solids 11 (5), 357–372. http://www.sciencedirect.com/science?_ob=ArticleURL&_udi=B6TXB-46G500N-… Log in or register to post comments Wed, 02/03/2010 - 03:25 Permalink
Ashwani Verma Representative Volume Element constitution dear Imechanica members i am looking for a help how can i constitute representative volume element to study fracture in hetrogeneous alloys. Ashwani Verma Ph D scholar Sant longowal Institute of Engineering & Technology, Longowal (INDIA) Log in or register to post comments Sun, 09/01/2013 - 04:40 Permalink
Hua Wang In reply to Representative Volume Element constitution by Ashwani Verma related book there are many works is related to your question. I think you should read the book about micro-mechanics Log in or register to post comments Wed, 09/25/2013 - 13:33 Permalink
Representative Volume Element (RVE)
JUAN GOMEZ
PhD Computational Mechanics
Professor
Applied Mechanics Group
EAFIT University
Medellin,Colombia
In reply to Representative Volume Element (RVE) by juan gomez
Hill (JMPS, 1963)
Please check the following reference:
Hill, R., 1963. Elastic properties of reinforced solids: some theoretical principles. J. Mech. Phys. Solids 11 (5), 357–372.
http://www.sciencedirect.com/science?_ob=ArticleURL&_udi=B6TXB-46G500N-…
Representative Volume Element constitution
dear Imechanica members
i am looking for a help how can i constitute representative volume element to study fracture in hetrogeneous alloys.
Ashwani Verma
Ph D scholar
Sant longowal Institute of Engineering & Technology, Longowal (INDIA)
In reply to Representative Volume Element constitution by Ashwani Verma
related book
there are many works is related to your question.
I think you should read the book about micro-mechanics