Submitted by dineshk on Wed, 12/31/2008 - 05:50 HI. I am doing project using ansys.can anyone help me how to analyse functionally graded material using ansys software Forums Ask iMechanica kouider84 ANALYSIS OF FUNCTIONALLY GRADED plateL USING ANSYS hello I am doing project using ansys. can anyone help me how to analyse functionally graded material using apdl ansys ; by the way i wonn study the harmonic vibration Log in or register to post comments Wed, 04/30/2014 - 10:11 Permalink Frank Richter FGM Hello, here are a few links on spatial variation of material properties Most of them explain the definition in Abaqus, their transfer to Ansys should be feasible 1) get this PhD thesis: DYNAMIC STRESS INTENSITY FACTORS FOR HOMOGENEOUS AND NONHOMOGENEOUS MATERIALS USING THE INTERACTION INTEGRAL METHOD BY SEONG HYEOK SONG THESIS Submitted in partial fulfillment of the requirements for the degree of Master of Science in Civil Engineering in the Graduate College of the University of Illinois at Urbana-Champaign, 2003 The code appears also in Buttlar, W., Paulino, G., and Song, S. (2006). ”Application of Graded Finite Elements for Asphalt Pavements.” J. Eng. Mech., 132(3), 240–249. Application of Graded Finite Elements for Asphalt Pavements 2) http://www.imechanica.org/node/9485 Varying material properties spatially in ABAQUS 3) http://www.imechanica.org/node/614 Functionally Graded Materials 4) SIMULIA Learning Community http://www.3ds.com/products-services/simulia/academics/simulia-learning… Defining Depth Dependent Material Properties in Abaqus by: Jessica NICHOLSON, 2013-10-17 5) http://paulino.cee.illinois.edu/software.html Development of user subroutines in commercial software (UMAT and UEL in ABAQUS) 6) a former reply in the ABAQUS mailing list http://groups.yahoo.com/neo/groups/Abaqus/info ---------------------------------------------------- Changing material property over coordinates You should be able to define your elastic modulus values as a tabular function of a field variable (set the number of field variables to "1" when defining an elastic material in the "Edit Material" dialog box). In this case, the field variable value will correspond to your Y-coordinate. Unfortunately, ABAQUS/CAE doesn't currently support the definition of predefined field variables (even though it has tools to define discrete and analytical fields which can be used in interaction and load definitions). So, you'll need to edit the input file to add a *INITIAL CONDITIONS,TYPE=FIELD,VARIABLE=1 section and/or a *FIELD,VARIABLE=1 section to actually define the field variable values. Alternatively, you can use the UFIELD subroutine (this might actually be easier, since the coordinates of the nodes are passed into the subroutine, and all you'll have to do is set FIELD(NSECPT,1) = COORDS(2)). Regards, Dave ------------------------- Dave Lindeman Lead Research Specialist 3M Company 3M Center 235-3F-08 St. Paul, MN 55144 651-733-6383 S.M.Ali Tasaloti wrote: > > > Hello to all, > Maybe my question is easy but I didn't find any answer for it. I want > for example to change the young modulus of material linearly over > y-coordinate of the 2D model. ---------------------------------------- Regards Frank ------------------------------------------ Ruhr-University Bochum Germany Log in or register to post comments Wed, 04/30/2014 - 12:19 Permalink Log in or register to post comments12461 views
kouider84 ANALYSIS OF FUNCTIONALLY GRADED plateL USING ANSYS hello I am doing project using ansys. can anyone help me how to analyse functionally graded material using apdl ansys ; by the way i wonn study the harmonic vibration Log in or register to post comments Wed, 04/30/2014 - 10:11 Permalink
Frank Richter FGM Hello, here are a few links on spatial variation of material properties Most of them explain the definition in Abaqus, their transfer to Ansys should be feasible 1) get this PhD thesis: DYNAMIC STRESS INTENSITY FACTORS FOR HOMOGENEOUS AND NONHOMOGENEOUS MATERIALS USING THE INTERACTION INTEGRAL METHOD BY SEONG HYEOK SONG THESIS Submitted in partial fulfillment of the requirements for the degree of Master of Science in Civil Engineering in the Graduate College of the University of Illinois at Urbana-Champaign, 2003 The code appears also in Buttlar, W., Paulino, G., and Song, S. (2006). ”Application of Graded Finite Elements for Asphalt Pavements.” J. Eng. Mech., 132(3), 240–249. Application of Graded Finite Elements for Asphalt Pavements 2) http://www.imechanica.org/node/9485 Varying material properties spatially in ABAQUS 3) http://www.imechanica.org/node/614 Functionally Graded Materials 4) SIMULIA Learning Community http://www.3ds.com/products-services/simulia/academics/simulia-learning… Defining Depth Dependent Material Properties in Abaqus by: Jessica NICHOLSON, 2013-10-17 5) http://paulino.cee.illinois.edu/software.html Development of user subroutines in commercial software (UMAT and UEL in ABAQUS) 6) a former reply in the ABAQUS mailing list http://groups.yahoo.com/neo/groups/Abaqus/info ---------------------------------------------------- Changing material property over coordinates You should be able to define your elastic modulus values as a tabular function of a field variable (set the number of field variables to "1" when defining an elastic material in the "Edit Material" dialog box). In this case, the field variable value will correspond to your Y-coordinate. Unfortunately, ABAQUS/CAE doesn't currently support the definition of predefined field variables (even though it has tools to define discrete and analytical fields which can be used in interaction and load definitions). So, you'll need to edit the input file to add a *INITIAL CONDITIONS,TYPE=FIELD,VARIABLE=1 section and/or a *FIELD,VARIABLE=1 section to actually define the field variable values. Alternatively, you can use the UFIELD subroutine (this might actually be easier, since the coordinates of the nodes are passed into the subroutine, and all you'll have to do is set FIELD(NSECPT,1) = COORDS(2)). Regards, Dave ------------------------- Dave Lindeman Lead Research Specialist 3M Company 3M Center 235-3F-08 St. Paul, MN 55144 651-733-6383 S.M.Ali Tasaloti wrote: > > > Hello to all, > Maybe my question is easy but I didn't find any answer for it. I want > for example to change the young modulus of material linearly over > y-coordinate of the 2D model. ---------------------------------------- Regards Frank ------------------------------------------ Ruhr-University Bochum Germany Log in or register to post comments Wed, 04/30/2014 - 12:19 Permalink
ANALYSIS OF FUNCTIONALLY GRADED plateL USING ANSYS
hello
I am doing project using ansys. can anyone help me how to analyse functionally graded material using apdl ansys ; by the way i wonn study the harmonic vibration
FGM
Hello,
here are a few links on spatial variation of material properties
Most of them explain the definition in Abaqus, their transfer to Ansys should be feasible
1) get this PhD thesis:
DYNAMIC STRESS INTENSITY FACTORS
FOR HOMOGENEOUS AND NONHOMOGENEOUS MATERIALS
USING THE INTERACTION INTEGRAL METHOD
BY
SEONG HYEOK SONG
THESIS
Submitted in partial fulfillment of the requirements
for the degree of Master of Science in Civil Engineering
in the Graduate College of the
University of Illinois at Urbana-Champaign, 2003
The code appears also in
Buttlar, W., Paulino, G., and Song, S. (2006). ”Application of Graded Finite Elements for Asphalt Pavements.” J. Eng. Mech., 132(3), 240–249.
Application of Graded Finite Elements for Asphalt Pavements
2) http://www.imechanica.org/node/9485
Varying material properties spatially in ABAQUS
3) http://www.imechanica.org/node/614
Functionally Graded Materials
4) SIMULIA Learning Community
http://www.3ds.com/products-services/simulia/academics/simulia-learning…
Defining Depth Dependent Material Properties in Abaqus
by: Jessica NICHOLSON, 2013-10-17
5) http://paulino.cee.illinois.edu/software.html
Development of user subroutines in commercial software (UMAT and UEL in ABAQUS)
6) a former reply in the ABAQUS mailing list
http://groups.yahoo.com/neo/groups/Abaqus/info
----------------------------------------------------
Changing material property over coordinates
You should be able to define your elastic modulus values as a tabular
function of a field variable (set the number of field variables to "1"
when defining an elastic material in the "Edit Material" dialog box).
In this case, the field variable value will correspond to your
Y-coordinate. Unfortunately, ABAQUS/CAE doesn't currently support the
definition of predefined field variables (even though it has tools to
define discrete and analytical fields which can be used in interaction
and load definitions). So, you'll need to edit the input file to add a
*INITIAL CONDITIONS,TYPE=FIELD,VARIABLE=1 section and/or a
*FIELD,VARIABLE=1 section to actually define the field variable values.
Alternatively, you can use the UFIELD subroutine (this might actually
be easier, since the coordinates of the nodes are passed into the
subroutine, and all you'll have to do is set FIELD(NSECPT,1) = COORDS(2)).
Regards,
Dave
-------------------------
Dave Lindeman
Lead Research Specialist
3M Company
3M Center 235-3F-08
St. Paul, MN 55144
651-733-6383
S.M.Ali Tasaloti wrote:
>
>
> Hello to all,
> Maybe my question is easy but I didn't find any answer for it. I want
> for example to change the young modulus of material linearly over
> y-coordinate of the 2D model.
----------------------------------------
Regards
Frank
------------------------------------------
Ruhr-University
Bochum
Germany