hello everyone,
I model a reinforced concrete column in ansys . ( with william-warkne criteria )
During Bending Loading the below error was appear .
Please guide me That Error What's meaning ?
*** FATAL *** CP = 93.507 TIME= 12:07:01
The supplied nonlinear material properties produced an incorrect
material tangent matrix. Please check your TB input carefully. A
very small yield stress may cause this failure.
Regard .
| Attachment | Size |
|---|---|
| File.txt | 12.48 KB |
Forums
I am currently trying to
I am currently trying to find a solution to the same problem. If you find anything, please post. I will do the same.
Thank you
I believe that the problem
I believe that the problem you are experiencing is that the first point in your MISO curve does not match exactly with the data point you entered for EX for the linear isometric material property. You may find that the solution to your problem to match exactly the first point of the MISO curve to coincide with modeled Young's modulus. Try this and post whether it works or not.
I am currently trying
I am currently trying to find a solution to the same problem. If you find anything, please post. I will do the same.Thank you!
My email address is duzibocumt [at] 163.com (duzibocumt[at]163[dot]com)。
In reply to I am currently trying by duzibocumt
Hi all! Have you solved this
Hi all! Have you solved this "fatal error" problem? I have the same difficulties with my modell (reinforced semi preacast slab in case of erection).
--> nonlinear concrete (Miso) Ex=30000N/mm2, first point= 9/Ex, 9 [N/mm2]. So this doesnt cause this exit fatal error.
Any suggestions? (its my master thesis)
Hi! Have you solved this
Hi! Have you solved this "fatal error" problem? I have the same difficulties with my modell (reinforced semi preacast slab in case of erection).
--> nonlinear concrete (Miso) Ex=30000N/mm2, first point= 9/Ex, 9 [N/mm2]. So this doesnt cause this exit fatal error.
Any suggestions? (its my master thesis)