Hi all,
One of our recent works on nanoscale directional motion induced by stiffness gradient.
I hope you will find it interesting.
http://dx.doi.org/10.1103/PhysRevLett.114.015504
This work has been presented in 2014 MRS Spring Meeting by Prof. Huajian Gao (the PPT file he used is attached): https://mrsspring14.zerista.com/event/member/109225
Best,
Tienchong
| Attachment | Size |
|---|---|
| 2014MRS_NDT.ppt | 11.03 MB |
Directional transport of molecular mass on graphene by straining
Dear Tienchong,
Thanks for sharing this interesting work!
We recently explored a potential mechanism of directional transport of molecular mass on graphene by straining, which is recently published in Extreme Mechanics Letters. Hope you find it interesting. The paper is now free to access at:
http://www.sciencedirect.com/science/article/pii/S2352431614000170
In reply to Directional transport of molecular mass on graphene by straining by Teng Li
It is interesting. Thanks.
It is interesting. Thanks.
statistical interlayer vdW potential
Dear Tienchong,
Thanks for sharing this excellent work!
I have a quick question to Figure 4(a) of your paper. Is the interlayer potential shown here a statistical/time-averaged value?
Look forward to your feedback!
Best wishes,
Shuze
In reply to statistical interlayer vdW potential by Shuze Zhu
Sure. It is. The calculation
Sure. It is. The calculation procedure was documented in the supplemental materials of our paper.