Skip to main content

Small values problem on Fatigue life cycles

Submitted by mmalekan on

Dear All,

I'm performing a fatigue life analysis of some standard specimens. The problem is I always get very small values (less than 1e-5) for the number of load cycles for each step of crack propagation! I used Paris and NASGRO formulas, but quite the same results. The SIF calculations are wroking correctly, since I'm using a commercial code to do that and I did double checked them to see if they are accurate enough. So, only Paris or NASGRO's parameters may bring some errors. But, I got them from the literature, for example: c = 1e-13 and m = 3.2 for Al 7075-T6. It's a simple caculation, don't know what exactly causes the problem!

Any advice would be greatly appreciated,

Mohammad

Paris law is what Barenblat calls incomplete similarity, nothing really fundamental.  They work in limited sense, may depend on specimen size, on R ratio, on microstructure, even on size of the crack!

Paul Paris was really fortunate to make a big career out of this finding --- after his paper was rejected 3 times by journals, he was in high demand of aeronautical companies who would fly him around.  Billions of dollars have been spent on "damage tolerance", and yet I am not sure it is really working.  Insurance companies do not like to hear about "cracks" anyway any longer, and so today "damage tolerance" is no longer very fashionable.  Are you still using it?

Ciavarella, Michele, Marco Paggi, and Alberto Carpinteri. "One, no one, and one hundred thousand crack propagation laws: a generalized Barenblatt and Botvina dimensional analysis approach to fatigue crack growth." Journal of the Mechanics and Physics of Solids 56, no. 12 (2008): 3416-3432.

Pugno, N., Ciavarella, M., Cornetti, P., & Carpinteri, A. (2006). A generalized Paris’ law for fatigue crack growth. Journal of the Mechanics and Physics of Solids, 54(7), 1333-1349.

Sat, 01/28/2017 - 19:36 Permalink