Submitted by qiuyifa on Tue, 07/03/2007 - 01:34 Dear Friends. I want to simulte the mechanic behavior of of Fiber Reinforced Composites and Textile Reinforced Composites. Could you give me some advice on which software is suitable? Thank you in advance Eric qiu Forums Materials Forum ramdas chennamsetti R. Chennamsetti, R&DE(E), R. Chennamsetti, R&DE(E), INDIA Hi Eric, Now a days all the commercial FE softwares like ANSYS and ABAQUS have special elements like layered SHELL and SOLID for simulating fiber reinforced composites (FRC). You may use any on of these softwares for simulating FRCs. - Ramdas Log in or register to post comments Sat, 07/07/2007 - 09:18 Permalink Log in or register to post comments4888 views
ramdas chennamsetti R. Chennamsetti, R&DE(E), R. Chennamsetti, R&DE(E), INDIA Hi Eric, Now a days all the commercial FE softwares like ANSYS and ABAQUS have special elements like layered SHELL and SOLID for simulating fiber reinforced composites (FRC). You may use any on of these softwares for simulating FRCs. - Ramdas Log in or register to post comments Sat, 07/07/2007 - 09:18 Permalink
R. Chennamsetti, R&DE(E),
R. Chennamsetti, R&DE(E), INDIA
Hi Eric,
Now a days all the commercial FE softwares like ANSYS and ABAQUS have special elements like layered SHELL and SOLID for simulating fiber reinforced composites (FRC). You may use any on of these softwares for simulating FRCs.
- Ramdas