Dear friends,
Can anybody give me information/Website/papers/... on below mentioned topic ??
on Johnson Cook plasticity model with analytical forms of the hardening law and rate dependence. I am trying to use this in my high-strain-rate transient dynamic simulations (metals). I am using ABAQUS as analysis tool.
Thanks a ton in advance !
-Balappa Bhairnatti.
Tooltech Deutschland
Munich.
Re: Johnson-Cook flow stress model
You can find some details of the model and some references in
http://www.eng.utah.edu/~banerjee/Papers/CuPlasticCompare.pdf
In reply to Re: Johnson-Cook flow stress model by Biswajit Banerjee
Johnson Cook model
Dear Biswajit Banerjee,
Thanks a lot for this information.
Have a nice day.
-Balappa. Bhairnatti.