i have to model a graphite/epoxy [0/+-45/90]2s composite laminate using ansys. can anyone please help me how to model it, as i m using ansys 4 the 1st time and dont know how to model a composite.
You may choose SHELL99 element. This is a layered shell element. Define the fiber orientation, material properties and thickness for each lamina in Real constants. Go through element library (help) before using this element.
I don't know whether this element is available in ANSYS 4 or not??? You may check in higher versions.
Ramdas is right, the SHELL99 element allows you to model composite materials. Before meshing you have to pay special attention to the element coordinate system been used. Normally for simple problems, using mesh attributes you can set an ESYS that is in conformity with the layer orientation. You can check the link here for more info.
Check this layer definition for a [90 0 90]s laminate, though one can define a symmetry option I think is better to define the whole set of layers. Tensile and shear modulus are defined in material properties, fiber volume fraction is not introduced as it is a parameter related to these tensile modulus. Thickness can be set for each different layer in RMODIF.
when we create a model for composite laminate, do we have to create each layer separately and then glue it together, or simply we just define the thickness and angles in real constant and model a simple one layer model having all the properties of layers. if so, how we can check the behavior of individual layers.
You don't have to create each layer separately since you are already defining them within the SHELL99 properties using real constants. This definition would be the one that characterizes laminate's response. Afterwards, you can use the command LAYPLOT to check visually the layer setting. Further postprocessing includes choosing a layer to display results with the command LAYER,n. You can choose if you want results in the top of that layer: SHELL, Top, or in the bottom: SHELL, Bot. It's recommended at this point to display results using the coordinate system of the active layer: RSYS, Solu.
can u plz tell me how to apply a tensile load of 20 lb/sec with a total range of load 10,000 lbs on a bar end in ansys, i have chosen shell99 element and i have to find the point of failure in the notched bar and the maximum stress induced at that point.
I am working on FE Modelling of Composite (graphite-epoxy) hollow rectangular section
beam in Ansys. When I select beam 188 element, there is no need of
inputting real constants. Where do i put the initial values in
pre-processing????Pls do help me,,I am new to applying Composite
material in Ansys.....pls...
I want to apply some number of unidirectional CFRP lamina with different orientations and make a laminate plate. I have the in-plane properties of lamina only and in ANSYS I have to define other out-of-plane properties which I don’t have.
In general, lamina is assumed to be transversely isotropic. Number of independent constants required becomes five, because of the following relations.
E22 = E33
G12 = G13
E22 = 2G23(1+nu23)
nu12 = nu13
Since E22, G12 and nu12 are in-plane properties. Use above relations to get unknown properties. Only nu23 is not known. This is value is very close to matrix Poisson ratio. Use that value (=nu23).
Engr. Adeela Khan
Engr. Adeela Khan
SHELL 99 in ANSYS
You may choose SHELL99 element. This is a layered shell element. Define the fiber orientation, material properties and thickness for each lamina in Real constants. Go through element library (help) before using this element.
I don't know whether this element is available in ANSYS 4 or not??? You may check in higher versions.
- Ramdas
In reply to SHELL 99 in ANSYS by ramdas chennamsetti
thanks for ur suggestions.
thanks for ur suggestions. i will try and hope it works
Ramdas is right, the SHELL99
Ramdas is right, the SHELL99 element allows you to model composite materials. Before meshing you have to pay special attention to the element coordinate system been used. Normally for simple problems, using mesh attributes you can set an ESYS that is in conformity with the layer orientation. You can check the link here for more info.
hi, i followed shell99
hi,
i followed shell99 element 4 my graphite/epoxy composite laminate, but the problem i m having is how to provide these given values in ansys,
my data is
Typical properties for unidirectional graphit/epoxy [0/+-45/90]2s system at room temp.
longitudinal tensile modulus(ksi) 20300,
transverse tensile modulus(ksi) 1490,
shear modulus (ksi) 830,
poisson's ratio (major) 0.3,
fiber volume fraction 0.74,
average thickness (in) 0.005,
can u plz guide me towards this,
waiting for an early response
regards
Khan
Layer definition
Check this layer definition for a [90 0 90]s laminate, though one can define a symmetry option I think is better to define the whole set of layers. Tensile and shear modulus are defined in material properties, fiber volume fraction is not introduced as it is a parameter related to these tensile modulus. Thickness can be set for each different layer in RMODIF.
/PREP7
!PLATE UNDER UNIAXIAL LOAD
!Element definition: layers and materials
ET,1,SHELL99
KEYOPT,1,8,1
!Real Constants: Layers
R,1
RMODIF,1,1,6,0,0,0,0,0 !6 layers
RMODIF,1,13, 1,90,0.5e-3, !set table_position 1 layer_angle layer_thickness
RMODIF,1,16, 1,0,0.5e-3,
RMODIF,1,19, 1,90,0.5e-3,
RMODIF,1,22, 1,90,0.5e-3,
RMODIF,1,25, 1,0,0.5e-3,
RMODIF,1,28, 1,90,0.5e-3,
!Materials
MPTEMP,,,,,,,,
MPTEMP,1,0
MPDATA,EX,1,,200e9 !longitudinal tensile modulus
MPDATA,EY,1,,5.2e9 !transverse tensile modulus
MPDATA,EZ,1,,5.2e9 !EY=EZ plane stress
MPDATA,PRXY,1,,0.26 !Major Poisson's ratios
MPDATA,PRYZ,1,,0.26
MPDATA,PRXZ,1,,0.26
MPDATA,GXY,1,,3e9 !Shear modulus
MPDATA,GYZ,1,,3e9
MPDATA,GXZ,1,,3e9
MPTEMP,,,,,,,,
MPTEMP,1,0
In reply to Layer definition by Octavio A. Gon…
Engr. Adeela Khan
Engr. Adeela Khan
layering
hi,
when we create a model for composite laminate, do we have to create each layer separately and then glue it together, or simply we just define the thickness and angles in real constant and model a simple one layer model having all the properties of layers. if so, how we can check the behavior of individual layers.
waiting for an early response
regards
Khan
layering
Hi Adeela,
You don't have to create each layer separately since you are already defining them within the SHELL99 properties using real constants. This definition would be the one that characterizes laminate's response. Afterwards, you can use the command LAYPLOT to check visually the layer setting. Further postprocessing includes choosing a layer to display results with the command LAYER,n. You can choose if you want results in the top of that layer: SHELL, Top, or in the bottom: SHELL, Bot. It's recommended at this point to display results using the coordinate system of the active layer: RSYS, Solu.
Cheers,
In reply to layering by Octavio A. Gon…
Thanks alot. It has
Thanks alot.
It has really helped me alot.
Regards
Khan
tensile loading
hi,
can u plz tell me how to apply a tensile load of 20 lb/sec with a total range of load 10,000 lbs on a bar end in ansys, i have chosen shell99 element and i have to find the point of failure in the notched bar and the maximum stress induced at that point.
waiting 4 an early response
regards
Khan
I am working on FE Modelling
I am working on FE Modelling of Composite (graphite-epoxy) hollow rectangular section
beam in Ansys. When I select beam 188 element, there is no need of
inputting real constants. Where do i put the initial values in
pre-processing????Pls do help me,,I am new to applying Composite
material in Ansys.....pls...
how to define out of plane properties of lamina?
Hi friends,
I want to apply some number of unidirectional CFRP lamina with different orientations and make a laminate plate. I have the in-plane properties of lamina only and in ANSYS I have to define other out-of-plane properties which I don’t have.
Can anyone help me to solve the problem?
Thank you in advance.
Transversely isotropic
Hi,
In general, lamina is assumed to be transversely isotropic. Number of independent constants required becomes five, because of the following relations.
E22 = E33
G12 = G13
E22 = 2G23(1+nu23)
nu12 = nu13
Since E22, G12 and nu12 are in-plane properties. Use above relations to get unknown properties. Only nu23 is not known. This is value is very close to matrix Poisson ratio. Use that value (=nu23).
With regards,
- Ramadas
Thank you Ramadas. It
Thank you Ramadas. It was functional.
Hamid
modeling 3d composite in abaqus
Hi all,
I have to model a 3d layup composite rather than a shell type with ABAQUS.
I have difficulty assigning appropriat material properties to a 3d stress element.
Is there anyone who can help me?
Thank you in advance.
Hamid