Source truncation and exhaustion: Insights from quantitative in-situ TEM tensile testing

Source truncation and
exhaustion: Insights from quantitative in-situ TEM tensile testing’ by D.
Kiener and A.M. Minor (
http://dx.doi.org/10.1021/nl201890s)