Experimental Verification of Automated Design of Reinforced Concrete Deep Beams - 2012
Mon, 2012-09-24 12:34 - SIMULIA
In this paper an automated design technique using nonlinear finite element analysis is presented and validated with experiment for RCDBs. This nonlinear finite element automated design technique was used to design the reinforcement for a RCDB.