Hi all,
I have a problem with perfect-plasticity material model in Abaqus. I this simple 2D analysis, I am modeling a beam fixed at both ends and applying temperature loading on it that will cause yielding. The material model is perfectly plastic with,
*PLASTIC
4.85 E8, 0.0
The problem is, stresses go beyond yield limit (4.85 E8) which should not be the case for the perfectly-plastic material model. I would appreciate any comment/help/suggestion.
Regards,
Soner
| Attachment | Size |
|---|---|
| inp file | 21.3 KB |
perfect plasticity
modify the command to
*PLASTIC
4.85 E8, 0.0
4.85001E8, <a strain value that approximate "infinity">