We have published two papers on Ecoflex, a popular silicone polymer in recent days. The polymer is largely temperature- and strain rate-insensitive. It comes up with several Shore Hardnesses. We characterize five Shores and develop a novel Shore-dependent modelling framework
Mechanics of Materials >> https://www.sciencedirect.com/science/article/pii/S016766362030020X
Polymer Testing >> https://www.sciencedirect.com/science/article/abs/pii/S0142941820301185