An improved Carroll's hyperelastic model considering compressibility and its finite element implementation

Submitted by Acta Mechanicaโ€ฆ on

Journal Tittle: Acta Mechanica Sinica

Article Tittle: An improved Carroll's hyperelastic model considering compressibility and its finite element implementation

Author: Stephen Kirwa Melly, Liwu Liu, Yanju Liu, Jinsong Leng

 

Novelty/impact/significance

Improved the predictive capabilities of Carroll's model and demonstrated its finite element implementation for accurate simulation of elastomeric component behavior.

 

Scientific question

The inaccurate predictions of Carroll's model specifically in the equibiaxial loading mode has been solved.

 

Key of how

The original strain energy expression is modified to comply with the restriction that it should vanish at the undeformed configuration and a compressible term is added.

 

Major points

1. Carroll's model is improved by modifying the strain energy density expression.

2. Numerical and finite element predictions are compared with classical experimental data.

3. The modified version demonstrated superior predictive capabilities.

 

Funding of the work

 

1. National Natural Science Foundation of China (Grant Nos. 11632005 and 11672086).

 