Anisotropy and chirality create an interesting mechanical coupling – axial-shear coupling. This paper also reports a weak correlation of chirality with negative Poisson’s ratio and a directional negative and positive Poisson’s ratio of a tetra-achiral lattice.
For more information, you can check this paper:
https://www.sciencedirect.com/science/article/pii/S0264127521000368