Skip to main content

High-throughput discovery of metal oxides with high thermoelectric performance via interpretable feature engineering on small data

Submitted by nuaajsh on

Published in Materials Today Physics: https://www.sciencedirect.com/science/article/pii/S2542529324001330

In this work, we have proposed a data-driven screening framework combining the interpretable machine learning with high-throughput calculations to identify a series of metal oxides that exhibit both high-temperature tolerance and high power factors. Aiming at the problem of weak generalization ability of small data with power factors at high temperatures, we employ symbolic regression for feature creation which enhances the robustness of the model while preserving the physical meaning of features. 33 candidate metal oxides are finally targeted for high-temperature thermoelectric applications from a pool of 48,694 compounds in the Materials Project database. The Boltzmann transport theory is utilized to perform electrical transport properties calculations at 1,000 K. The relaxation time is approximated by employing constant electron-phonon coupling based on the deformation potential theory. Considering band degeneracy, the electron group velocity is obtained using the momentum matrix element method, yielding 28 materials with power factors greater than 50 μWcm−1K−2. The high-throughput framework we proposed is instrumental in the selection of metal oxides for high-temperature thermoelectric applications. Furthermore, our data-driven analysis and transport calculation suggest that metal oxides rich in elements such as cerium (Ce), tin (Sn), and lead (Pb) tend to exhibit high power factors at high temperatures.