Constitutive modeling of hyperelastic solids reinforced by spheroidal particles under large deformations

Submitted by rezaavaz on

This paper presents a homogenization-based constitutive model for the mechanical behavior of particle-reinforced elastomers with random microstructures subjected to finite deformations. The model is based on a recently developed homogenization method (Avazmohammadi and Ponte Castaneda 2013; J. Elasticity 112, 1828โ€“1850) for two-phase, hyperelastic composites, and is able to directly account for the shape, orientation, and concentration of the particles.