Surface Ripples of Polymeric Nanofibers under Tension: The Crucial Role of Poisson’s Ratio Submitted by Ying Li on Thu, 09/11/2014 - 02:10 research polymer fiber surface ripple dynamic instability finite element modeling Coarse-grained molecular dynamics Shan Tang, Ying Li, Wing Kam Liu and XiaoXu Huang Read more about Surface Ripples of Polymeric Nanofibers under Tension: The Crucial Role of Poisson’s Ratio2 commentsLog in to post comments6516 views