Journal Club Theme of January 2015: Topology Optimization for Materials Design

Submitted by Jamie Guest on

Processing technologies are rapidly advancing and manufacturers now have the ability to control material architecture, or topology, at unprecedented length scales. This opens up the design space and provides exciting opportunities for tailoring material properties through design of the materialโ€™s topology. But as seen many times in history with advancements in materials and processing technologies, the natural default is to rely on familiar shapes and structure topologies.