Spiral fracture in metallic glasses and its correlation with failure criterion
Xianqi Lei,Yujie Wei, Bingchen Wei, Wei-Hua Wang. Acta Materialia 99, 206-212 (2015). doi:10.1016/j.actamat.2015.08.008