Multiple pass accumulative rolling

Arun Prakash's picture

A multiscale simulation framework of the ARB process

The accumulative roll bonding process is one of the most prominent severe plastic deformation processes for obtaining sheet materials with ultra-fine-grained microstructures and high strength. The properties of such sheets differ significantly from those of conventionally rolled sheets. It is hence desirable to have a simulation framework that can accurately predict the material properties, including the evolving texture and anisotropy during processing.