Microstructural observations and tensile fracture behavior of FSW twin roll cast AZ31 Mg sheets

Defect-free joints were friction stir welded (FSW) from AZ31 Mg alloy sheets by employing optimum welding parameters for the tool geometry used. Microstructure, texture and mechanical response of the welded joints were studied to identify susceptibility of crack initiation in the different weld zones and to understand the overall fracture behavior of these welds.