Formation path of delta hydrides in zirconium by multiphase field modeling

Submitted by mohsenzaeem on

A multiphase field model is developed to study the effects of metastable ฮถ and ฮณ hydrides on the nucleation and growth of the stable ฮด hydrides in ฮฑ zirconium matrix.  Acta Materialia 123 (2017) 235-244