Superalloys; Dislocation microstructure evolution; Anti-phase boundary; Intrinsic size effects; Dislocation dynamics

The strength and dislocation microstructure evolution in superalloy microcrystals

Submitted by ahmed.hussein on

In this work, the evolution of the dislocations microstructure in single crystal two-phase superalloy microcrystals under monotonic loading has been studied using the three-dimensional discrete dislocation dynamics (DDD) method. The DDD framework has been extended to properly handle the collective behavior of dislocations and their interactions with large collections of arbitrary shaped precipitates. Few constraints are imposed on the initial distribution of the dislocations or the precipitates, and the extended DDD framework can support experimentally-obtained precipitate geometries.