Edge effect of strained bilayer nanofilms for tunable multistability and actuation

Inspired by the need to develop reconfigurable materials at the micro- and nano- scales that are capable of exhibiting more than one stable configuration, we employed both theoretical and computational models supported by experiments to study the multistable behavior of a Si/Cr microclaw and uncover the mechanical principles involved.