Atomistic modeling of out-of-plane deformation of a propagating Griffith crack in graphene. Submitted by Nuwan Dewapriya on Fri, 09/22/2017 - 13:14 research crack propagation fracture graphene crack surface deformation Griffith crack Abstract Read more about Atomistic modeling of out-of-plane deformation of a propagating Griffith crack in graphene.Log in to post comments2162 views