Steering with light: indexable photomotility in liquid crystalline polymers Submitted by Mahnoush Babaei on Thu, 02/08/2018 - 02:03 research Liquid Crystal Elastomers Photoactuation Photomotility DOI: 10.1039/C7RA10619J RSC Adv., 2017, 7, 52510-52516 Read more about Steering with light: indexable photomotility in liquid crystalline polymersLog in to post comments2424 views