The plausibility of <cโ€ฏ+โ€ฏa> dislocation slip on {-12-11} planes in Mg

Submitted by Yizhe_Tang on

Dear Colleagues,

Please see the link for a recent article published in Scripta Materialia. In this article, active cross-slip behavior of screw <c + a> dislocations in Mg is observed, and the plausibility of <c + a> dislocation slip on new planes {-12-11} that have hitherto not been considered possible, is shown for the first time.

Thanks to Elsevierโ€™s sharing policy, this article has 50 days' free access, and anyone can read and download it before August 30, 2018.