Mechanisms of compressive deformation and failure of porous bulk metallic glasses

Submitted by Parag Tandaiya on

Porous Bulk Metallic Glasses have been invented by researchers to mitigate catastrophic failure in monolithic Bulk Metallic Glasses which are susceptible to intense strain localization into shear bands.