#Fracture Toughness

Fracture of notched ductile bulk metallic glass bars subjected to tension-torsion: experiments and simulations

Submitted by Parag Tandaiya on

There is a shortage of literature on mode III fracture behaviour of bulk metallic glasses.

In our following research paper published in Acta Materialia, we report our experiments and three-dimensional elasto-plastic finite element simulations of tension-torsion loading on notched ductile bulk metallic glass bars.

It is found that fracture toughness of this BMG is lowest in mode II among all three fracture modes.

Temperature-dependence of mode I fracture toughness of a bulk metallic glass

Submitted by Parag Tandaiya on

Bulk Metallic Glasses were found to exhibit an intermediate temperature minimum in ductility. Does it also lead to an intermediate temperature minimum in fracture toughness?