Hydrolysis-induced large swelling of polyacrylamide hydrogels Submitted by Lihua Jin on Mon, 09/07/2020 - 14:49 research hydrogel reaction hydrolysis polyelectrolyte non-equilibrium thermodynamics By Yu Zhou and Lihua Jin Read more about Hydrolysis-induced large swelling of polyacrylamide hydrogelsLog in to post comments2482 views