Shear fracture in bulk metallic glass composites

In situ dendrite reinforced Bulk Metallic Glass matrix composites (BMGCs) are known to overcome poor ductility and fracture response exhibited by monolithic bulk metallic glasses (BMGs). In this paper (Shear fracture in bulk metallic glass composites) recently published by our group in Acta Materialia, we report mode I and mode II fracture experiments on the above in situ BMGCs containing transforming and non-transforming dendrites.