Smart Laser-Writable Micropatterns with Multiscale Photo/ Moisture Reconstructible Structure

Submitted by zichen on

The design of a dynamic, versatile, convertible, and responsive micropatterned system is realized by a photo/moisture reconstructible multiscale film-substrate bilayer structure. Specifically, a hydrophilic polyvinyl alcohol (PVA)/laponite (LP) thin film is covalently bonded to a photothermally active polydimethylsiloxane (PDMS)/carbon black (CB) soft substrate. A laser engraver can inscribe programmable aligned micro-wrinkles by manipulating laser power and spatiotemporal control.