Programmable 3D Self-Folding Structures with Strain Engineering

Submitted by zichen on

Self-assembly of three-dimensional (3D) structures, through bending, twisting, folding, and buckling, has garnered broad interest among physicists, mathematicians, chemists, and biologists. Herein strain engineering and geometric frustration as an on-demand strategy for fabricating spontaneous rolling โ€œorigamiโ€ structures with programmable multistability across multiple length scales are exploited.