Superelasticity and shape memory effect in zirconia nanoparticles
In this work, superelastic and shape memory properties of single crystalline and polycrystalline yttria stabilized tetragonal zirconia (YSTZ) nanoparticles are studied by atomistic simulations. N. Zhang and M. Asle Zaeem. Superelasticity and shape memory effect in zirconia nanoparticles. Extreme Mechanics Letters 46 (2021) 101301 (8 pages).