negative Poisson ratio

Luca-Deseri's picture

Bulky auxeticity, tensile buckling and deck-of-cards kinematics emerging from structured continua

Complex mechanical behaviours are generally met in macroscopically homogeneous media as effects of inelastic responses or as results of unconventional material properties, which are postulated or due to structural systems at the meso/micro-scale.

Examples are strain localization due to plasticity or damage and metamaterials exhibiting negative Poisson’s ratios resulting from special porous, eventually buckling, sub-structures.