Shock response of polymers
Our latest article โQuantum and classical molecular dynamics simulations of shocked polyurea and polyurethaneโ is available freely for 50 days from this URL: https://authors.elsevier.com/a/1eJem3In-urdzV
Highlights of the article are as follows:
โข Quantum molecular dynamics were used to compute shock Hugoniot data up to 75 GPa.
โข The shock response of polyurea and polyurethane are remarkably similar.