Submitted by Ramathasan Theโ€ฆ on

Abstract

 

Background: Helmet systems most commonly experience oblique blunt impacts which cause simultaneous linear and rotational accelerations. The ability to attenuate both linear and rotational accelerations by absorbing the normal shock while accommodating large shear deformations with energy dissipation is critical to developing superior helmet liners that prevent traumatic brain injury (TBI).