Finite strains explain the non-monotonic change of contact area in soft rubber contacts loaded in torsion?

In unidirectional sliding of rubber contacts on smooth hard surface it has been found that contact shrinks largely in longitudinal directions, and generally much less in the transverse direction, and two explanations have been suggested to explain this: one is the effect of mixed mode fracture mechanics in the presence of adhesion (with mode II reducing adhesion and mode III less clear), and another uniquely based on finite strain effects even for a simple material model as neo-Hookean hyperelastic material.