Skip to main content

Plywood- orthotropic material

I Would like to include failure in my model

Submitted by hdeepu25 on

I am doing my master thesis on crash simulation of plywood (7 layers-orthotropic material) structures in buses using explicit LS-DYNA FE program. I would like to include failure in my model. Right now I am working on Mat_054_55 (MAT_ENHANCED_COMPOSITE_DAMAGEโ€ฆ..material model from LS-DYNA material library).

 

Mat_054_55 allows me to get failure by defining anyone of the following parameters,